APPLICATION SCHEDULE
Ø Applied by electrostatic spraying gun that can provide negative tension of 60-80 kV.
Ø Curing schedule :10-15 minutes at 180-200℃ (metal temperature )
Ø Optimal film thickness : 70 - 90 um
POWDER PROPERTIES
Ø Specific gravity : 1.25 - 1.75 (depend on colors)
Ø Particle size distribution(Laser Particle size analyser) : Less than 5% above 100 um
50 – 65% above 32 um :
Average particle size : 35- 45um
SUBSTRATES AND PRE-TREATMENT
In order to obtain optimal anti-corrosion properties, it is recommended to apply a chemical pretreatment prior to powder coating application.
Ø Ferrous metals(cold rolled steel, cast iron etc.): Iron or zinc phosphatation
Ø Zinc surfaces(galvanized steel, zinc alloy) : Chromatation or zinc phosphatation
Ø Aluminum alloys : Chromatation
SORT BY CHEMISTRY:
Epoxy Powder Coating
Epoxy-Polyester/Hybrid
Polyester-TGIC
Polyester TGIC-Free
Polyurethane
SORT BY FINISH OR CHARACTERISTIC:
Anti-gassing Powder Coating Anti-graffiti Powder Coating
Antimicrobial Powder Coating Chrome Effect Powder Coating
Crocodile Skin Powder Coating High Temperature Resistant
Metallic/Peal Powder Coating Sublimation Powder Coating
Texture Effect Powder Coating Transparent Clear Topcoats
Wood Effect Powder Coating Zinc Rich Epoxy Primers
Why choose our products?
1). We have our own factory. The good quality and the competitive is the advantage of our company.
2). The material we choose is always good and products always come out with high quality.
3). A trial order or sample orders are welcomed.
4). Our products are exported to Europe, America, Southeast Asia, and other countries and regions in the world.
5). We will do our best to service you all the time if you have the further question.
Contact Information:
Ms. Susie Xie
Tel: 86 25 83313610 Mob/Whatsapp/Wechat: 86 17751006340