    1.
    Issues with the formulation design of the powder coating:
    • Insufficient heat resistance of pigmentsIf the heat resistance temperature of the pigments is not high enough, the powder coating may change color during the high-temperature baking process.

    • Poor thermal stability of resins and additivesSome resins, curing agents, and additives may undergo thermal decomposition at high temperatures, leading to unstable coating color.

    2.
    Problems with the selection of raw materials:
    • Improper selection of pigmentsChoosing pigments that are not light-resistant or have poor weather resistance can easily cause the coating film to change color under light or outdoor conditions.

    • Poor compatibility between resin and pigmentIf the compatibility between the resin and pigment is not good in the formulation design, floating color phenomenon may occur.

    3.
    Issues with the manufacturing process:
    • Insufficient pre-mixingIf the pigment distribution in the powder coating is uneven, it will lead to uneven coating color.

    • Improper extrusion, cooling, grinding, and other process parametersIf the temperature, pressure, time, and other parameters in these process steps are not properly controlled, it will also affect the color and quality of the powder coating.

    4.
    Issues with the application process:
    • Improper baking conditionsOver-baking or under-baking can cause the coating film to change color.

    • Volatile gases in the ovenThese gases may react with the coating film, causing discoloration.

    • Improper pre-treatmentResidual treatment liquid or inadequate treatment of the workpiece surface will affect the color and gloss of the coating film.

    5.
    Issues with the storage and transportation of powder coatings:
    • Exposure to moisture or heatIf the powder coating is exposed to moisture or heat during storage and transportation, it will affect its color and quality.

    6.
    Other factors:
    • Improper use of recycled powderIf the mixing ratio of recycled powder to new powder is improper, or if the quality of the recycled powder is poor, it will lead to changes in coating color.

    • Mixing of different powder coatingsMixing different types of powder coatings or powder coatings from different manufacturers can easily lead to inconsistent coating color.

Solutions

    1.Improve formulation designChoose pigments with good heat resistance, light resistance, and weather resistance, and resins, curing agents, and additives with good thermal stability.
    2.Strictly control the manufacturing processEnsure that the parameters in the pre-mixing, extrusion, cooling, grinding, and other process steps are properly controlled to ensure the quality stability of the powder coating.
    3.Optimize the application processDevelop appropriate baking conditions to avoid over-baking or the presence of volatile gases in the oven; improve the pre-treatment process to ensure the cleanliness of the workpiece surface.
    4.Proper storage and transportationAvoid powder coatings from being exposed to moisture or heat, and keep the storage environment dry and cool.
    5.Reasonable use of recycled powderControl the mixing ratio of recycled powder to new powder, and ensure the quality of the recycled powder.
    6.Avoid mixing of powdersThoroughly clean the powder spraying system before application to avoid mixing different types or different manufacturers of powder coatings.

Through the above measures, the problem of color fading and color differences in powder coatings after leaving the factory can be effectively reduced.